The density with the fabricated G centers along with the signal-to-sound ratios of personal emitters introduced a direct connection with the annealing problems as well [129], indicating a progressive dissociation on the defects together with a lower within the history sign for an extended annealing period. For that reason, off-equilibrium fabricati